Colored EVA Film for Glass Deep Processing

Product Details
Customization: Available
After-sales Service: 12 Months
Warranty: 12 Months
Still deciding? Get samples of US$ 1/Bag
Request Sample
Diamond Member Since 2024

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Importers and Exporters
The supplier has import and export rights
to see all verified strength labels (13)
  • Colored EVA Film for Glass Deep Processing
  • Colored EVA Film for Glass Deep Processing
  • Colored EVA Film for Glass Deep Processing
  • Colored EVA Film for Glass Deep Processing
  • Colored EVA Film for Glass Deep Processing
  • Colored EVA Film for Glass Deep Processing
Find Similar Products
  • Overview
  • Product Parameters
  • Detailed Photos
Overview

Basic Info.

Model NO.
GS38C
Type
Laminated Glass
Shape
Flat
Structure
Solid
Layer Type
Common Laminated Glass
Function
Decorative
Intermediate Film
EVA Film
Melting Point
High Temperature
Production
Dry Laminated Glass
Usage
Furniture, Door, Building, Window
Meltingpoint
67ºC
Density
0.951g
Glass Transition Temp
-45
Tensile Strength
31MPa
Elongation(Before Laminated)
774
Bonding Strength(Glass)
95n Every 10mm
Transport Package
Wooden Box
Specification
2.4*50m
Trademark
h&h
Origin
China
Production Capacity
50000

Product Description

Product Parameters

 

Technical parameters of vision colorful EVA film
 
Item Unit Performance index
Melting point ºC 67
Density g/cm3 0.951
Glass transition Temp ºC -45
Tensile strength Mpa 31
Elongation(before laminated) % 774
Water absorption % ≤0.1
Light transmittance % about 50
Bonding strength(glass) N/ 10mm 95
UV aging resistance(15Kwh/ m2,290~385nm) Light transmittance% 79.6
Damp&heat aging (85ºC 85%humidity 1000h) Light transmittance% 78.3
Impact resistance against shot-bag GB-15763.3-2009 1200MM Qualified
Ball inpact resistance GB-15763.3-2009 4800MM Qualified
Humidity aging resistance GB-15763.3-2009   Qualified



Technical   arameters of opague colorful EVA film
Item Unit Performance index
Melting point ºC 67
Density g/cm3 0.951
Glass transition Temp ºC -45
Tensile strength Mpa 31
Elongation(before laminated) % 774
Water absorption % ≤0.1
Light transmittance % about 0.3
Bonding strength(glass) N/ 10mm 95
UV aging resistance(15Kwh/ m2,290~385nm) Light transmittance% 79.6
Damp&heat aging (85ºC 85%humidity 1000h) Light transmittance% 78.3
Impact resistance against shot-bag GB-15763.3-2009 1200MM Qualified
Ball inpact resistance GB-15763.3-2009 4800MM Qualified
Humidity aging resistance GB-15763.3-2009   Qualified
Detailed Photos

 

Colored EVA Film for Glass Deep ProcessingColored EVA Film for Glass Deep ProcessingColored EVA Film for Glass Deep ProcessingColored EVA Film for Glass Deep ProcessingColored EVA Film for Glass Deep ProcessingColored EVA Film for Glass Deep Processing

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier